abstract |
Provided are an antireflection film that has both ease of finger sliding and transparency, and a method for manufacturing the antireflection film. An antireflection film 10 includes a substrate film 12 and a first resin layer 14 formed over a surface of the substrate film 12, and the first resin layer 14 contains large particles 18 that form raised portions in a surface of the first resin layer 14, hollow silica particles 22 that have a smaller average particle size than the large particles 18, and a binder resin. The amount of the large particles 18 is preferably within a range of 1.0 to 3.5 mass% of the total mass of the first resin layer 14, and the amount of the hollow silica particles 22 is preferably within a range of 30 to 70 mass% of the total mass of the first resin layer 14. |