abstract |
The invention relates to a method for producing a treated object, comprising the steps: a) producing an object by means of additive manufacturing, the object being produced by the repeated arrangement, layer by layer, of at least one first material on a substrate spatially selectively in accordance with a cross-section of the object, the method comprising the additional method step: b) at least partially bringing the object, which is still on the substrate or has already been detached from the substrate and which has been produced by additive manufacturing, into contact with a liquid heated to ≥ T or a powder bed of a second material heated to ≥ T for a time ≥ 1 minute in order to obtain the treated object, T standing for a temperature of ≥ 25 °C. The invention further relates to an object produced by a method of this type. |