abstract |
The present invention relates to a polyol component comprising a1) a polyol having a weight averaged molecular weight Mw of from 1,000 to 4,000 Dalton, a number averaged molecular weight Mn of from 600 to 2,500 Dalton, an OH value between 80 and 300 mg KOH / g of resin and a glass transition temperature Tg of from -10 to 90 °C, and a2) between 0.1 and 10 % by weight of polyurea product as rheological agent, as well as it use in a crosslinkable composition especially suitable for clear coat applications. |