http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-3677653-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_527d41cad118be2c39e19a33eab54468 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D133-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D101-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D101-02 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D101-02 |
filingDate | 2017-08-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fef2e9722dd46c978465be3cd0349064 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_693022a88f8f91911ac12de6eddd87f7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d3f877f7ccbf84d0ba29a081f57ab9fd http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6907841bdc78d7a2999e3a29dfdf7094 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9886c19b2ef7cb9a899d48e900d3a060 |
publicationDate | 2020-07-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | EP-3677653-A1 |
titleOfInvention | Fibrous-cellulose-containing composition and coating |
abstract | It is an object of the present invention to provide a cellulose fiber-containing composition and a cellulose fiber-containing paint, the particles (aggregates) of which are suppressed in coated products. According to the present invention, provided is a cellulose fiber-containing composition comprising cellulose fibers having a fiber width of 1000 nm or less and water, wherein the image clarity (comb width: 0.125 mm) of a coating film obtained from the following conditions is 55% or more:(Conditions)the cellulose fiber-containing composition, an acrylic resin in an amount of 156 parts by weight based on 1 part by weight of the cellulose fibers, and isocyanate in an amount of 44 parts by weight based on 1 part by weight of the cellulose fibers, are mixed with one another to obtain a coating solution, which is then applied onto a smooth polyethylene terephthalate plate to a thickness of 30 µm, using an applicator, and immediately after the application of the coating solution, it is dried at 80°C for 30 minutes. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11591481-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-3660159-A4 |
priorityDate | 2017-08-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 294.