abstract |
Provided is a molded article which contains a first enclosure; a second enclosure adjoined with the first enclosure; and a transparent member held by the second enclosure, each of the first enclosure and the second enclosure being independently made from a resin composition that contains a polyamide resin having a semi-crystallization time of 10 to 60 seconds, and a melting point of 200 to 280°C, and the transparent member having a pencil hardness of 8H or larger, and a linear expansion coefficient of 1×10<sup>-6</sup>to 9×10<sup>-6</sup>/°C, where the semi-crystallization time means a time measured by depolarization photometry at a temperature 20°C higher than the melting point of the polyamide resin, for a melting time of polyamide resin of 5 minutes, and at a temperature of crystallization bath of 150°C. |