Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_387abf6afc9a2cd5cfa5cd4d35f8b9fe |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G2350-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2312-00 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-17 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-3206 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-3271 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-7671 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-797 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-6696 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-4829 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L75-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-05 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-48 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-66 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-79 |
filingDate |
2017-09-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9ea9c5a567e35fc36ccd4fed46489bdb http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d1fe287d0d4af750740bed0602b298f0 |
publicationDate |
2019-08-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
EP-3519476-A1 |
titleOfInvention |
Resin composition for damping materials |
abstract |
[Problem] The present invention is to provide a composition which can easily form a polyurethane resin which exerts particularly excellent damping properties in an operating temperature range. [Solution to Problem] A resin composition for damping materials, including a polyol-containing component (A) and a polyisocyanate (B), in which the polyol-containing component (A) contains a castor oil and in which when the composition is cured, the peak on its Tan δ curve is 0.7 or more and the temperature for the peak is in a range of -10°C to 100°C. |