http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-3315277-A1

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c97f90ab12b35b650d5fd039ed7a41a5
classificationCPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G01N21-648
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29L2011-00
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G01N21-648
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C33-3842
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G01N21-64
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G01N21-41
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C33-38
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C33-38
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G01N21-41
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G01N21-64
filingDate 2016-06-17-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_421dd656b32d6c717d038c2a15637502
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2174efacbc5423b7f1484c2ab2ad3fd7
publicationDate 2018-05-02-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber EP-3315277-A1
titleOfInvention Forming mold, optical element, and method for producing optical element
abstract There is provided a forming mold made on the basis of a standard more reliable than an average roughness of a surface of a metal film that generates surface plasmon resonance, the forming mold being capable of improving an S/N ratio of an optical element. A forming mold 40 includes a fixed mold 41 and a movable mold 42. A molding surface 51t is provided at a tip end of a core section 51 of the fixed mold 41. When an Spc value of the molding surface 51t is equal to or less than 100 (1/mm), the state of a surface 21a of a substrate 21, on a side facing an object to be measured, obtained by transferring the molding surface 51t can be made smooth to the extent that the generation of a scattering light in a metal film 22 to be formed on this surface 21a can be appropriately suppressed. Thus, it is possible to improve an S/N ratio in the measurement using Surface Plasmon-field enhanced Fluorescence Spectroscopy. In contrast, when the Spc value of the molding surface 51t is equal to or greater than 30 (1/mm), the molding surface 51t can be relatively easily machined and a plasmon resonance angle for increasing a signal level can be easily detected.
priorityDate 2015-06-25-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID323
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID54230877
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID226422866
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID226397779

Total number of triples: 24.