abstract |
The present invention aims to provide a polyester polyol having favorable reactivity and a favorable color tone, which can be used for obtaining a polyurethane having an excellent balance of flexibility, mechanical strength, and chemical resistance, and a method for producing the polyester polyol. The object can be achieved with a polyester polyol in which an aliphatic diol contains as a structural unit 1,10-decanediol derived from a biomass resource, and in which the aldehyde body content in the polyester polyol is 0.01 to 0.5% by weight, and a method for producing the polyester polyol. |