Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_0ddb9f3656270bc5410be3679322fead |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2006-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2006-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G21K5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B2204-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B2204-04 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05H6-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05H3-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B32-205 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K5-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G21K5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B32-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G21G4-02 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G21K5-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H05H6-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C14-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01B32-182 |
filingDate |
2015-12-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d1796445e063ba17e107e08bd93cdd8e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4a3a5bec1106fa85dd0e752fd79c8eb8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_349dcb3d555147752b4c171d7978a86e |
publicationDate |
2017-10-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
EP-3228591-A1 |
titleOfInvention |
Interlayer thermally bondable graphite sheet for high vacuum |
abstract |
The object of the present invention is to provide a material which has an excellent thermal conductivity as a thermal interface material even under the condition of high vacuum and has no risk of contaminating the interior of an apparatus and outgassing. The present invention is characterized in having a thickness of not more than 9.6 µm and not less than 50 nm and a thermal conductivity in the a-b surface direction at 25°C of not less than 1000 W/mK. It is preferred that a density be not less than 1.8 g/cm 3 in the present invention. The graphite sheet of the present invention is preferably obtained by thermally treating a polymer film at a temperature of not less than 2900°C. The polymer film is preferably at least one kind selected from among polyamides, polyimides, polyquinoxalines, polyoxadiazoles, polybenzimidazoles and the like. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-3496111-A4 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11581105-B2 |
priorityDate |
2014-12-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |