Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c1755eede76ea7e719a3e0d2843cd793 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2201-026 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2205-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2423-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2201-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2423-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2323-12 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-0061 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L21-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-103 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J9-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J3-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J3-28 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L21-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-16 |
filingDate |
2015-09-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a0e370c5bc3d357ba9d0c91bb9ef2d38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8ff511db49db58b0043f7610544fd0fe |
publicationDate |
2017-08-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
EP-3202832-A1 |
titleOfInvention |
Crosslinked polyolefin foam |
abstract |
A crosslinked polyolefin foam that is a crosslinked foam of a polyolefin resin composition, the composition comprising a polyolefin resin (A) and a rubber (B) having a Mooney viscosity (ML 1+4 , 100°C) of 15 to 85. The rubber (B) is contained in an amount of 10 to 150 parts by mass relative to 100 parts by mass of the polyolefin resin (A). The foam has a thickness of 1.5 mm or more, a 25% compressive hardness of 60 kPa or less, and a crosslinking degree of at least one of surface layers at both surfaces with a depth of 500 µm from the surface that is at least 5% higher than the crosslinking degree of the middle layer excluding the both surface layers. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11680145-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-3604411-A4 |
priorityDate |
2014-09-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |