Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e5ad8562c578b061df7a2c3aee9d0e24 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W30-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2363-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2300-24 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J7-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J11-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J11-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J11-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J11-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J11-20 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J11-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J7-02 |
filingDate |
2016-10-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7ec3f28ef45db4f427717ba4fde70f3b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4182844ae6d7b0027338bb96a31d42eb http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c7720db4042a1528c9f07e037abffbbb http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_16829962e01a5c40008f160b90bd3094 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_62eafecc08630ad3f9bb9b993b7df1ba http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_691cf606bb02afb37715670328b095fd http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cb53064fe89b0e0120ccba006ee643a5 |
publicationDate |
2017-04-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
EP-3153543-A1 |
titleOfInvention |
Method and composition for swelling pretreatment before decomposition of cured thermosetting resin materials |
abstract |
Provided are a composition for swelling pretreatment of a cured thermosetting resin material before decomposition, including a surfactant and an acidic material, and a method for swelling pretreatment of a cured thermosetting resin material before decomposition by using the same. When carrying out swelling pretreatment of a cured thermosetting resin material before decomposition by using the composition, it is possible to accelerate infiltration of the acidic material into the cured thermosetting resin material and swelling of the cured thermosetting resin material by virtue of the surfactant, and thus to increase the decomposition reactive surface area. Therefore, it is possible to increase reaction efficiency during the subsequent decomposition process, and to increase the decomposition ratio during the same period of time. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2019008685-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2019008685-A1 |
priorityDate |
2015-10-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |