abstract |
A composite molded body, and its manufacturing method, is provided wherein the composite body contains a layer comprising a copolymer of tetrafluoroethylene (TFE) and perfluoro(ethyl vinyl ether) (PEVE). The composite body can be manufactured under conditions in which an adjoined layer of thermoplastic resin and/or thermosetting resin is not be melted, thermally degraded or decomposed. The copolymer has a PEVE content of 20 to 80 weight percent, based on the total weight of the copolymer, and a melt flow rate of from 0.1 to 100 g/10 min, as measured in compliance with ASTM D1238 at a temperature of 250°C ± 0.1 using a 5 kg weight. |