Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_034ebbaf6b674882d63102f499e29056 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J2479-02 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J179-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D21H17-07 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D21H17-56 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D21H17-72 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L79-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D21H17-15 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G73-0286 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D21H21-146 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21H17-55 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21H17-46 |
filingDate |
2014-11-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b597bf67c64592bc9e2cc59c8aef9b92 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_38529d66bb9b521034cf3b7ea1df1224 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e1356eec588634ec61dfefe916374302 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f465a8bcd16a749fe9b80294bbff75e4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_98a592c1a7bfb3bcd4381e0d4b2e0e86 |
publicationDate |
2016-09-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
EP-3066261-A1 |
titleOfInvention |
Creping adhesives and methods for making and using same |
abstract |
Creping adhesives and methods for making and using same are provided. The creping adhesive can include a first thermosetting polyamidoamine-epihalohydrin resin that includes a reaction product of a first epihalohydrin and a first polyamidoamine containing one or more secondary amine groups, a first thermoplastic polyamidoamine-epihalohydrin resin that includes a reaction product of a second epihalohydrin and a second polyamidoamine containing one or more secondary amine groups, and one or more re-wetting agents. The first thermosetting polyamidoamine-epihalohydrin resin can have a weight average molecular weight of about 800,000 to about 1,200,000 and a molar ratio of the first epihalohydrin to the secondary amine groups of about 0.002:1 to about 0.1:1. The first thermoplastic polyamidoamine-epihalohydrin resin can have a weight average molecular weight of about 40,000 to about 200,000 and a molar ratio of the second epihalohydrin to the secondary amine groups of about 0.001:1 to about 0.1:1. |