Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_f37f4ff2c8f3ec7c2dd049ff046cc2ac |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B41C1-1066 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B41N1-086 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B41N1-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B41N1-083 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41C1-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41N1-08 |
filingDate |
2014-11-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_80e99c8c8e9a064b3b2d377c6cd87851 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a34e8bf1477c1d08d2d51f0f8632b721 |
publicationDate |
2016-05-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
EP-3017943-A1 |
titleOfInvention |
A sustainable lithographic printing plate |
abstract |
A method of preparing a lithographic printing plate comprises the steps: printing a liquid on a lithographic support thereby forming a printing area which corresponds to a raster image; and where the printing area is characterized by having a maximum thickness between 2.0 and 50.0 µm |