http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-2940066-A1

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_4efb7acb6b26fa9d42d6a70c99ed5b15
classificationCPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2867-003
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29L2007-008
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2995-002
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2089-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2389-00
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C07K14-43518
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L89-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C71-02
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C55-02
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J5-18
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C39-02
classificationIPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L7-00
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L89-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C71-02
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C55-02
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C39-02
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07K14-435
filingDate 2013-12-17-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b0a4518273b05d3d982ca1e88c0a032f
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_14e972c61109ab7714df63cb0b28d9c6
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d0a77d94d437a6a3aac355c165d65e7b
publicationDate 2015-11-04-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber EP-2940066-A1
titleOfInvention Spider silk protein film, and method for producing same
abstract A film of the present invention contains a polypeptide derived from spider silk proteins. The decomposition temperature of the film is 240 to 260°C. The film absorbs ultraviolet light having a wavelength of 200 to 300 nm and has a light transmittance of 85% or more at a wavelength of 400 to 780 nm. The film is transparent and colorless in a visible light region. A method for producing a film of the present invention includes: dissolving a polypeptide derived from spider silk proteins in a dimethyl sulfoxide solvent to prepare a dope; and cast-molding the dope on a surface of a base. Thus, the present invention provides a spider silk protein film that can be formed easily and has favorable stretchability, and a method for producing the same.
priorityDate 2012-12-26-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID128833854
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID13529
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID11263
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID226413548
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID12695
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID129453277
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID6249
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID656894
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID145742
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID226395685
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID127548652
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID127584974
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID127965897

Total number of triples: 42.