Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_bbd1d44888f5b41142d83de455096387 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2982 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82Y15-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10S977-896 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2004-53 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2004-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2004-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2004-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2004-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01G5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2006-90 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2006-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2006-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2006-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10S977-957 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T436-173845 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82Y40-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2004-64 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10S977-773 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G01N33-52 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01G7-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01G7-00 |
filingDate |
2014-02-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6ed62025079908ed90f4400753e49e8f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8abb74252fe24696f08e106cbe80cd95 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4bb9bdb2b3de549e091c8472b0ff820e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_91cc085fce428caeb43b6b472c3ddae8 |
publicationDate |
2015-08-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
EP-2905259-A1 |
titleOfInvention |
Porous noble metal oxide nanoparticles, method for preparing the same and their use |
abstract |
The present invention discloses a method for preparing porous noble metal oxide nanoparticles, comprising the following steps: a) preparing an Olea Europaea fruit extract; b) preparing an Acacia Nilotica extract; c) mixing the Olea Europaea fruit extract and the Acacia Nilotica extract for preparing a mixed extract; d) providing an aqueous solution containing a noble metal compound dissolved therein; e) mixing the mixed extract obtained in step c) and the aqueous solution of step d); f) dropping a solution of sodium chloride to be mixture of step b); d) drying the mixture, in air or by vacuum, and h) calcining at a temperature between 100 to 900°C, to get the porous noble metal oxide nanoparticles; porous noble metal oxide nanoparticles obtained thereby and their use. |