Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_78ca80ad4b743c901ec136b21263f093 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L71-123 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L51-04 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L53-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L55-02 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L51-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L71-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-00 |
filingDate |
2013-09-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6264f7bd010ec3191b4bce5326f4602f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_475b2be96316b6be5bcc72ed424c4f71 |
publicationDate |
2015-07-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
EP-2898019-A1 |
titleOfInvention |
Poly(phenylene ether) composition and article |
abstract |
A composition includes 15 to 35 weight percent of a poly(phenylene ether) having an intrinsic viscosity of 0.29 to 0.43 deciliter per gram, and 65 to 85 weight percent of a rubber modified polystyrene. The composition exhibits improved heat resistance relative to acrylonitrile-butadiene-styrene copolymer (ABS) while maintaining comparable levels of melt flow, impact resistance, and tensile strength. Articles such as electrical housings can be molded from the composition. |