Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7f9af914ed2fb00cd4f1b8b1a28964e4 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J27-1853 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J27-1817 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J35-023 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J37-0201 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J37-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J27-1856 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J27-1804 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J27-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J37-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J37-031 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C07C45-52 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J37-088 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J27-1806 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07C45-29 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J27-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07B61-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07C47-22 |
filingDate |
2011-03-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_18a028ca841f85c054f64cac77076b91 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0cad75191f4e825f97364c088f0ce216 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_92dbfc6e0228363618524a670bb27116 |
publicationDate |
2015-06-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
EP-2886193-A2 |
titleOfInvention |
Catalyst for glycerin dehydration, and process for producing acrolein, process for producing acrylic acid, and process for producing hydrophilic resin each using the catalyst |
abstract |
A catalyst for glycerin dehydration of the present invention comprises a rare-earth metal phosphate, wherein a molar ratio P/R of phosphorus (P) to a rare-earth metal (R) is more than 1.0 and 2.0 or less. An another catalyst for glycerin dehydration of the present invention comprises a combination of a rare-earth metal phosphate and a metal element other than a rare-earth metal, wherein a molar ratio M/(P+R) of a metal element (M) to phosphorus (P) and a rare-earth metal (R) is more than 0.00005 and 0.5 or less. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112619699-A |
priorityDate |
2010-03-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |