http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-2735002-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_fab5a78161702097f97524ce6e5cdcd7 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C18-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01B1-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C18-143 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01B1-22 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B1-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B1-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-24 |
filingDate | 2012-07-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e4ab0d88e2e0cca7dc9b3f10a20cbe8b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_21ec0f1aff822fa42b2cf0e007439b94 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_952e4e72f4f29678050996a07edc8de5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0ed71d6278f52af259b194c760f887bd |
publicationDate | 2014-05-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | EP-2735002-A1 |
titleOfInvention | Method for producing thin electrically conductive layers of silver, a silver layer, a silver complex, the solution of said silver complex, and the use of the silver complex in a solution |
abstract | The invention relates to a method for producing thin electrically conductive layers of silver on a surface of substrates, electrically conductive layers, a silver complex and a solution of the silver complex, and also the use of a silver complex solution. In a method for producing thin electrically conductive layers of silver on a surface of substrates, in a first method step, silver nitrate and 2-pyrrolidone are dissolved in a solvent, preferably water or an ethanol/water mixture, and in the process [Ag(Pyl)2]NO3 is formed by complexing. In a second method step, the solution is applied to a surface of the substrate which is to be coated and then, in a third method step, chemical reduction, which leads to the separation of silver from the other contained chemical components, is carried out by irradiation with electromagnetic radiation from the wavelength spectrum of UV light over a period of at least 15 minutes. Then, in a fourth method step, heat treatment at a temperature of at most 500°C, preferably at 220°C, is carried out over a period of at least 30 minutes, preferably 60 minutes, and in the process a layer which is formed at least virtually exclusively from silver is obtained on the surface of the substrate. |