http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-2711392-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_18a8284bc1d41fe092e46c249d6220be |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-12 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J4-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-10 |
filingDate | 2012-09-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d50a1305960a74089a457db8756f3aa9 |
publicationDate | 2014-03-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | EP-2711392-A1 |
titleOfInvention | Process for the preparation of a composition comprising heterophasic propylene copolymer and talc |
abstract | The invention relates to a process for the preparation of a composition comprising a heterophasic propylene copolymer, a propylene copolymer and talc, wherein the heterophasic propylene copolymer consists of (a) a propylene-based matrix, wherein the propylene-based matrix consists of a propylene homopolymer and/or a propylene- α-olefin copolymer consisting of at least 70% by mass of propylene and up to 30% by mass of α-olefin based on the total mass of the propylene-based matrix, wherein the propylene-based matrix is present in an amount of 60 to 95wt% based on the total heterophasic propylene copolymer nand (b) a dispersed ethylene-α-olefin copolymer, wherein the dispersed ethylene-α-olefin copolymer is present in an amount of 40 to 5wt% based on the total heterophasic propylene copolymer and wherein the sum of the total amount of propylene-based matrix and total amount of the dispersed ethylene-α-olefin copolymer in the heterophasic propylene copolymer is 100wt%, wherein the composition has a desired melt flow index in the range of 1 to 200dg/min as measured according to ISO1133 (2.16 kg/230°C) comprising the steps of (a) melt-mixing a propylene copolymer with a talc to obtain a masterbatch (b) melt-mixing the masterbatch with the heterophasic propylene copolymer and a peroxide to obtain the composition comprising a heterophasic propylene copolymer, a propylene copolymer and talc, wherein the amount of peroxide is chosen such that a composition comprising a heterophasic propylene copolymer, a propylene copolymer and talc having the desired melt flow index is obtained. |