abstract |
Nickel-chromium-manganese alloy with 0.005 to 0.07% by weight of carbon, 20.5 to 23.0% by weight of chromium, 0.05 to 1.5% by weight of silicon, 1.5 to 6.0% by weight of manganese, 1.7 to 3.0% by weight of nickel, 0.15 to 0.30% by weight of nitrogen, 0.1 to 0.8% by weight of molybdenum, 0.05 to 4.5% by weight of copper, up to 0.3% by weight Cobalt, up to 0.04% by weight of phosphorus, up to 0.04% by weight of sulfur, up to 0.2% by weight of niobium, up to 0.2% by weight of vanadium, up to 0.2% by weight of zirconium, up to 0.2% by weight of tungsten, to 0.2% by weight of tantalum, to 0.1% by weight of lead, to 0.1% by weight of bismuth, to 0.1% by weight of tin, to 0.1% by weight of zinc, to 0.1% by weight of selenium, to 0 , 1 wt% arsenic, up to 0.1 wt% titanium, up to 0.05 wt% aluminum, up to 0.05 wt% calicum, up to 0.05 wt% magnesium, up to 0.05 wt% barium, up to 0.05 % By weight of lanthanum, up to 0.05% by weight of cerium, up to 0.05% by weight of yttrium, up to 0.05% by weight of rhenium, up to 0.05% by weight of oxygen, up to 0.05% by weight of boron, balance iron, including impurities caused by melting. |