Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8e0bf0928b608797b70bbc2b91c7e52e |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L67-02 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F6-92 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L67-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01D5-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F6-84 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01D5-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-92 |
filingDate |
2011-10-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7afb01edea002e0135ec198afdffaca6 |
publicationDate |
2013-09-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
EP-2632985-A1 |
titleOfInvention |
Use of polymer blends for producing slit film tapes |
abstract |
The present invention relates to the use of polymer blends for producing slit film tapes comprising: A) 30% to 50% by weight of a biodegradable, aliphatic-aromatic polyester; B) 50% to 70% by weight of polylactic acid and C) 0% to 2% by weight of a compatibilizer. |
priorityDate |
2010-10-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |