Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_26828a7eaa10755e15e8498759e41017 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J2231-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J2531-822 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J31-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J31-181 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J31-165 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F4-027 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F4-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F26-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J31-08 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J31-20 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F26-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J31-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J37-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J35-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-18 |
filingDate |
2012-02-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9abd0a7244efff32b2f64d58d0ef1d29 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6229a87640ac7ce4f08b0e9602f7d432 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_91679b1730c0d5ea4fbaca99a71da326 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_14d0280ebaa8f655453cd409271173a0 |
publicationDate |
2013-08-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
EP-2631010-A1 |
titleOfInvention |
Vinylpyridine resin for catalyst carriers and method of manufacturing the same |
abstract |
A vinylpyridine resin that is hardly pulverized and thermally decomposed such that the degradation of the catalytic activity is suppressed while having a pore volume and a specific surface area to maintain a sufficient catalytic activity, and also a method of manufacturing the vinylpyridine resin are provided. The resin represents: a volume ratio of the pores having a diameter of 3 through 5 nm to all the pores of not less than 4% and not more than 60%; a total pore volume of not less than 0.15 cc/g and not more than 0.35 cc/g; and a specific surface area of not less than 20 m 2 /g and not more than 100 m 2 /g. The resin can be manufactured by using a combination of a poor solvent, such as octane and not less than 50 wt% and not more than 90 wt% of a good solvent, in particular a compound having a benzene ring such as toluene, as porous agent. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-108778496-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-108778496-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2017159466-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11065607-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111848931-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111848931-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-3747540-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/TW-I642480-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2017159466-A1 |
priorityDate |
2012-02-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |