http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-2604633-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_0ddb9f3656270bc5410be3679322fead |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F20-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F4-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F220-1804 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F4-50 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F20-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-40 |
filingDate | 2011-07-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c30aa7a83bbef3d9264223acf1ababdb http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fcac3d93d8d9f5be661b0e2c566ccc69 |
publicationDate | 2013-06-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | EP-2604633-A1 |
titleOfInvention | Manufacturing method of (meth) acrylic polymer |
abstract | In the conventional living radical polymerization process that uses a transition metal complex catalyst, in order to allow polymerization to proceed to a high monomer conversion rate and thereby obtain a polymer having a narrow molecular weight distribution when a reducing agent is used together and the amount of transition metal atoms of the transition metal complex is set to 30 ppm or less, it has been necessary to use a multidentate amine in excess relative to the transition metal. In addition, a method has been disclosed which allows polymerization to proceed even when the amount of multidentate amine is small, by adding an amine as a reducing agent; however, the reaction velocity is slow and thus it is difficult to achieve a high monomer conversion rate. However, in a method for polymerizing a (meth)acrylic monomer by living radical polymerization in the presence of a transition metal complex catalyst, the combined use of a multidentate amine (A), a base (B) and a reducing agent (C) makes it possible to achieve a rapid polymerization reaction and high monomer conversion rate and obtain a polymer having a narrow molecular weight distribution when 5-30 ppm by weight of copper atoms and a mole amount of 7 mmol% or less of multidentate amine (A) are used, each based on the total amount of (meth)acrylic monomer introduced. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2015004171-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-2824117-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8883941-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105358585-A |
priorityDate | 2010-08-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 184.