http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-2542645-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d6660167441edb2ac3d2d8445b278307 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01J61-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K11-77 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K11-7777 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K11-02 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K11-77 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01J61-44 |
filingDate | 2011-02-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f05d32f093d753bd2acd83aa3e3eb0a1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5af0d0368f8a73d630c9c43963667104 |
publicationDate | 2013-01-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | EP-2542645-A1 |
titleOfInvention | Core-shell phosphor produced by heat-treating a precursor in the presence of lithium tetraborate |
abstract | The phosphor of the invention is characterized in that same is capable of being produced by a method in which a precursor including particles having an average diameter of between 1.5 and 15 micrometers is heat-treated under a reducing atmosphere, said particles including a mineral core and a shell containing a composite phosphate of lanthanum and/or cerium, optionally doped with terbium, which covers the mineral core uniformly over a thickness greater than or equal to 300 nm, the heat treatment taking place in the presence of lithium tetraborate (Li2B4O7), as a fluxing agent, in a mass quantity of at most 0.2%, at a temperature of between 1050°C and 1150°C and for a time period of between 2 hours and 4 hours. |