abstract |
To provide a water/oil repellent composition which is capable of imparting sufficient dynamic water repellency to the surface of an article, has high stability of the particles of the copolymer, and presents a low environmental impact, a method for its production, and a method for treating an article. A water/oil repellent composition comprising a copolymer (A) having structural units based on a monomer (a) having a C 1-6 polyfluoroalkyl group, structural units based on a (meth)acrylate (b) having a Z20-30 alkyl group and structural units based on a halogenated olefin (c), a surfactant (B), and a medium (C), wherein the medium (C) comprises water and a propylene glycol type solvent, and the amount of the propylene glycol type solvent is from 35 to 80 parts by mass per 100 parts by mass of the copolymer (A). |