http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-2398854-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_4fdd0beb7f8c1b60c08cb52ec2a2dcb1 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L61-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L61-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L61-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L61-28 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L61-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L61-20 |
filingDate | 2010-02-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a94514e78189628c2781277fb0075b7f |
publicationDate | 2011-12-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | EP-2398854-A1 |
titleOfInvention | Improved polymer preparation |
abstract | The invention provides a retarded acid-curing pre-polymeric composition wherein the composition comprises an acid, a pre-polymer and hydroxylamine; use of hydroxylamine as a retarder for an acid-curing pre-polymer composition; a method of retarding the curing of an acid- curing pre-polymeric composition which method comprises the step of adding hydroxylamine to the pre-polymer to form a pre-polymer mixture; and a method of curing a retarded acid-curing pre-polymeric composition wherein the method comprises the step of heating the composition to an elevated temperature for use in improving processing and controlling reactivity in a wide range of industrial applications. |
priorityDate | 2009-02-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |