Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ac31afbea1cbbb03498644721ffb4a62 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B7-323 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B7-04 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B7-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B7-04 |
filingDate |
2010-07-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e32212d47715ab40a4610263df4bbd8e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5ae2d6c41af7154080618ffa0efb8bb4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_81f6a05ae9a5c8ecb7abd46ea331d8ad http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e1c5758b43125967e58977316de62664 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8346d9e656b63f14e1b77355555258b5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bb3097794cc431845edf5ea727fcc53c |
publicationDate |
2011-08-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
EP-2357161-A1 |
titleOfInvention |
Method for secondarily synthesizing calcium sulphoaluminate mineral in portland cement clinker |
abstract |
A method for secondarily synthesizing calcium sulphoaluminate mineral in Portland cement clinker is provided. The method includes adding plaster into raw Portland cement and calcination, then heating twice to re-form calcium sulphoaluminate mineral that is decomposed at high temperature in the clinker. This method can increase the content of calcium sulphoaluminate mineral in the clinker, sufficiently exert the advantages of the calcium sulphoaluminate mineral in the clinker, enhance the early stage performance and long-term performance of the cement clinker, and increase the quantity of mixture in the cement. |