http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-2350169-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c0c22533c7d145dac1210effc398763c |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L101-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L63-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2351-06 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J3-11 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F8-46 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D151-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J3-246 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F10-06 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D151-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-11 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D123-14 |
filingDate | 2009-11-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0f8d30ef6a81dce81c469aebd3d3e704 |
publicationDate | 2011-08-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | EP-2350169-A1 |
titleOfInvention | Polymer dispersions of narrow particle size distribution |
abstract | A process for the manufacture of a polymer dispersion comprising the steps of i) providing a mixture comprising from 2 to 60 parts by weight of a first polypropylene polymer having sufficient carboxylic acid and/or carboxylic acid anhydride groups equivalent to an acid value of from 2 to 50 mg KOH/g nv polymer and from 40 to 98 parts by weight of a second polymer having a molar excess of functional groups capable of reacting with the carboxylic acid and/or carboxylic acid anhydride groups of the polypropylene ii) causing the polymers to melt at a chosen temperature under conditions of high shear in an extruder to form an intimate mixture of the polymers iii) causing some of the carboxylic acid and/or carboxylic acid anhydride groups of the polypropylene to react with at least some of the functional groups of the second polymer to form a reaction mixture, under conditions of high shear in an extruder iv) rapidly cooling the reaction mixture outside the extruder to form a solid product v) optionally breaking up the solid product into smaller pieces vi) contacting the solid product with an organic liquid wherein the organic liquid is chosen to be a good solvent for the second polymer and a poor solvent for the polypropylene polymer whereby a dispersion comprising polypropylene particles in a solution of the second polymer dissolved in the organic liquid is formed. |
priorityDate | 2008-11-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |