Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_268be9afa00cf55b5aa72b1612151ecb |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25D11-18 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25F7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25D7-0635 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25F3-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B41N3-034 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25D7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25D7-0607 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25D11-024 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25D11-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25D11-005 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25F7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25F3-04 |
filingDate |
2009-09-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c2581c7f260b53a3097e1e87bdce9137 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ed4cf47033191a9a3e2314f3a6b4d8b8 |
publicationDate |
2011-07-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
EP-2343402-A1 |
titleOfInvention |
Electrolytic treatment method and electrolytic treatment device |
abstract |
An electrolytic treatment method and electrolytic treatment device are provided for electrolytic treatment of an aluminum web W by applying an alternating current to an upstream electrode 6A and a downstream electrode 6B disposed along a conveying direction a. At least one of a conveying velocity v of the aluminum web W, a frequency f of alternating current applied at the upstream electrode 6A and the downstream electrode 6B, and/or a web conveying direction separation distance d2 between the upstream electrode 6A and the downstream electrode 6B are set such that the alternating current and voltage waveform applied to the aluminum web W at the far end of the upstream electrode 6A and the alternating current and voltage waveform applied to the aluminum web W at the near end of the downstream electrode 6B do not reinforce each other. |