http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-2258669-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7e3c990dc67c29a8cfb71a9db599f13d http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b216734bf5922a9e9891858c6a8a0c10 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B28-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B28B13-0275 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B28B7-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B28B21-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F04B15-023 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B28B1-54 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B12-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B28-36 |
filingDate | 2009-03-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_766e1e881453f73fc579aae4778a70ec http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_172ecf625c0ee94b4494f3e0c6e22bea http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f7988854221e47d1b5cdc8adb3fdec0c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_720d5c0e25d61d81404888acf216ba38 |
publicationDate | 2010-12-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | EP-2258669-A1 |
titleOfInvention | Production method and production system of solidified sulfur |
abstract | In the present invention, a sulfur-containing material in a melt state is stored in material hopper 1 heated to a temperature within a preset temperature range of which a lower limit is equal to or above a melting point of sulfur. The stored sulfur-containing material is sucked by pressure generators 2a, 2b and pulled out into cylinders 11a, 11b heated to a temperature within the preset temperature range. The pulled out sulfur-containing material is pushed out from the cylinders under predetermined pressure applied by the pressure generator, and thereafter, the resultant material is injected from injection port 24 into mold 5 having therein a cavity which can be hermetically sealed and the mold being heated to a temperature within the preset temperature range. The injection port of the mold after the sulfur-containing material is fully injected in the cavity is closed. By stopping heating of the mold, the sulfur-containing material injected in the cavity is slowly cooled. After that, a modified sulfur concrete substance formed by cooling and solidifying the sulfur-containing material in the cavity is taken out from the mold. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/IT-MI20110668-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8894720-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2012143388-A3 |
priorityDate | 2008-03-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 62.