Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_574bc8fd24e08fc5a292d012c5a28e48 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B2519-02 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B37-06 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B37-06 |
filingDate |
2009-02-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_259e6229e5d7d3147df0dbdfa8f428aa http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_69238ba64748a26375a6018bcf4813bc |
publicationDate |
2010-08-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
EP-2218579-A1 |
titleOfInvention |
Improved method for manufacturing a laminated multi-layer film |
abstract |
The present invention relates to a method for producing a laminated layer composite, in which at least one base layer (3) and at least one further layer (4), between which a component (1) is located, consists of two thermoplastic materials with different Vicat softening temperatures B / 50 laminated in two stages to form a laminate. The invention furthermore relates to a layer structure suitable for this process, to a laminated layer composite produced by this process, and to a security and / or value document containing such a laminated layer composite. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2023285358-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-3501819-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-104896211-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11731411-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2019121278-A1 |
priorityDate |
2009-02-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |