Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_9592efd24c0c67b5f1b405d7d0c0c29a |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2666-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L9-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2666-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2666-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-3435 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-139 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-005 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-005 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L9-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L53-025 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L53-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F16L9-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-3435 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-142 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-17 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L25-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L9-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L53-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F16L9-12 |
filingDate |
2008-02-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2010-10-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8232397cc96a0edc13dbebf9ca535dd2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_58894f5cd2311c88ffb56c16bd54d721 |
publicationDate |
2010-10-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
EP-2110409-B1 |
titleOfInvention |
Piping member formed by using propylene resin composition |
abstract |
Disclosed is a piping member formed by using a propylene resin composition having a melt flow rate after kneading of 0.01-2.00 g/10 minutes. The propylene resin composition essentially contains (A) 100 parts by mass of a propylene-ethylene random copolymer having an ethylene content of 2-5%, a crystallization temperature of 86-105˚C, a melt flow rate of 0.01-2.00 g/10 minutes, and a molecular weight distribution of 3-8, and (B) 1-15 parts by mass of a styrene-butadiene rubber having a styrene content of 10-40% and a weight average molecular weight of not less than 200,000. This propylene resin composition is characterized by further containing (C) 0.1-1.0 part by mass of a hindered amine light stabilizer having a weight average molecular weight of not less than 2,000 per 100 parts by mass of the propylene-ethylene random copolymer. Also disclosed is a piping member formed by using such a propylene resin composition which is characterized in that the styrene-butadiene rubber is composed of a hydrogenated styrene-butadiene copolymer rubber. |