abstract |
The invention relates to filled polycarbonate compositions with modified resilience containing A) 10 - 90 parts by wt. of aromatic polycarbonate and/or aromatic polyester carbonate, B) 0.5 - 30 parts by wt. of rubber-modified graft polymer, C) 0. 1 - 50 parts by wt. of hollow glass balls, D) 0 - 20 parts by weight of a flame-proofing agent containing phosphorus, E) 0 - 40 parts by weight of vinyl(co)polymer (E.1) and/or polyalkylene terephthalate (E.2), and F) 0 - 10 parts by weight of other additives. Said compositions are characterised by having an improved flow behaviour, a high stiffness and low processing shrinkage and its high scratch resistant properties remain unchanged. The invention also relates to a method for the production thereof, to the use thereof for producing moulded bodies and moulded bodies that can be obtained from the above-mentioned compositions. |