http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-1993700-A2

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_74c93cc6b2ff4c69f0cb70d77ae21e68
classificationCPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F23K2201-505
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D2257-602
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T436-12
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D2253-106
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D2253-104
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F23J2215-60
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W90-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P90-90
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F23J7-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G06Q40-12
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F23J15-003
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F23K1-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G06Q10-30
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D53-83
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01D45-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01D46-00
filingDate 2007-01-17-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d1bcbcd24f3e42e9c46210ad4c989dbd
publicationDate 2008-11-26-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber EP-1993700-A2
titleOfInvention Methods of operating a coal burning facility
abstract Methods involve adding sorbent components, such as calcium oxide, alumina, and silica, as well as optional halogens as part of environmental control. Use of the sorbents leads to significant reductions in sulfur and mercury emissions that otherwise would result from burning coal. Use of the sorbents leads to production of waste coal ash that, while higher in mercury, is nevertheless usable as a commercial product because the mercury in the ash is non-leaching and because the coal ash has a higher cementitious nature by virtue of the increased content of the sorbent components in the ash. Thus, the methods involve adding powders having qualities that lead to the production of a cementitious coal ash while at the same time reducing emissions from a coal burning facility.
priorityDate 2006-01-18-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID127739328
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID127854467
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID3024
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID5558
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID6332
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID129112787

Total number of triples: 31.