Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_758994071efb42b565fc2c04637be131 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2998 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2991 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J3-126 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L31-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L75-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-098 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-51 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-42 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-12 |
filingDate |
2006-04-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_88470f9a7139bb3c3c728f074d6190b2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a4276d0661a18404021dd2008bc76e8f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_63413edf99a36b5a4887b7b6da98c1dc |
publicationDate |
2008-02-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
EP-1887027-A1 |
titleOfInvention |
Resin particle and resin dispersion |
abstract |
Resin particles which are excellent in electrostatic property, thermal storage stability and thermal properties, and have evenness of particle diameter are to be provided. The resin particles are core-shell resin particles (C2) each comprising one or more film-like shell layers (P) comprising a first resin (a) and a core layer (Q) comprising a second resin (b). Core-shell type resin particles (C2) each comprising a film-like shell layer (P) in one or more layer structure comprising a first resin (a) and a core layer (Q) in one layer structure comprising a second resin (b), wherein the weight ratio of (P) and (Q) is in a range of (0.1:99.9) to (70:30), the content of volatile components of (C2) is 2% by weight or lower, and (a) has an initial softening temperature of 40 to 270°C, a glass transition temperature of 20 to 250°C, a flow temperature of 60 to 300°C, and the difference of the glass transition temperature and the flow temperature in a range of 0 to 120°C and contains 20 to 80% by weight of vinyl acetate as constituent units. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10626355-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-3093317-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-1932860-A4 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2019002682-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-1932860-A1 |
priorityDate |
2005-04-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |