Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_268be9afa00cf55b5aa72b1612151ecb |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B41M5-506 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B41M5-504 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D21H19-84 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03C1-79 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G7-006 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B41M5-502 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B41M5-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G7-004 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B7-10 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21H27-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21H27-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21H25-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-775 |
filingDate |
2006-01-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_93ad0be90a05e771f87d52bd7936cbf9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_661b2f8f50dd98596de2f059713240b6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7dc761af0c7bb9fc835c877a1f1caf08 |
publicationDate |
2007-12-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
EP-1867474-A1 |
titleOfInvention |
Support for image recording material, process for producing the same, and image recording material |
abstract |
The present invention provides an image-recording material support having high surface smoothness and excellent gloss, a method for producing the same and an image-recording material using the image-recording material support. n To this end, the present invention provides a image-recording material support which has a raw paper and a polymer coating layer on both surfaces of the raw paper, wherein the raw paper has a value of tensile energy absorption (TEA) in the CD direction/basis weight of 1,000mJ/g to 2,100mJ/g and is subjected to a soft calender treatment such that a surface of the raw paper on which an image is to be recorded makes contact with a roller having a surface temperature of 200°C to 350°C. |