Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_9398da123a8c8c2a49c888d51704728a |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2105-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2105-12 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-767 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/E04F13-083 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-07 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-022 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C48-2886 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/E04F13-0864 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C48-07 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C48-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C48-395 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C48-76 |
filingDate |
2005-11-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_82bc709e7014c34f9c327104eadc7619 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b674cf6fe9e4ad54704727961f98f3be http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7616990f900a808b407f2ef8deff7cdb http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4b2dc740cb3fa657828a9584e59a9c86 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ccc64768e2dbf089b0ddf80af4b0016f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a71fdd69a633c13527121ae2df173e87 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6c4924727abf0c42f00582cc14a08662 |
publicationDate |
2007-08-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
EP-1812219-A1 |
titleOfInvention |
Wet use chopped strand glass as reinforcement in extruded products |
abstract |
A method for incorporating wet use chopped strand glass (WUCS) in a screw extrusion process is provided. A polymeric resin is added to an extruder (100) in a polymer feed zone (106) and conveyed to a first compression zone (113) where the resin is at least partially melted. The molten resin is conveyed to a high volume zone (107) where WUCS fibers are added. In the high volume zone, the flights of the screw may have a greater pitch to facilitate the introduction of the WUCS into the extruder. The molten resin/fiber mixture is conveyed to a second compression zone (112) where the resin and fibers are intimately compounded. Next, the molten resin/fiber mass is conveyed to a low pressure zone (115) where moisture evaporated from the fibers is released through an opening (109). The resin/fiber mixture is then conveyed through a compression/die feed zone (116) to further compound and mix the resin and fibers. |
priorityDate |
2004-11-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |