abstract |
Composite particles having a BET surface area of 5 to 100 m 2 / g containing a zinc oxide matrix and cerium oxide domains, wherein the domains are in and on the matrix and the proportion of zinc oxide is 80 to 98 wt .-% and the proportion to cerium oxide 2 to 20 wt .-%, each based on the composite particles is. |