abstract |
A method for producing a highly crystalline perovskite-type complex compound is provided that exhibits stably a high Seebeck coefficient and a low electric resistivity even at higher temperatures. A method for producing a complex perovskite-type compound with less environmental load is also provided. The method comprises a step of dissolving a nitrate salt containing a rare earth element, a nitrate salt containing an alkaline earth metal element, a nitrate salt containing manganese, and an organic polymer into a solvent to form a solution, a step of mixing and stirring the solution, a step of preparing a precursor powder from the solution through heating and drying thereof, and a step of calcining the precursor powder in atmosphere. |