http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-1741752-B1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e443fcd44793752f156437bbfd4c8603 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-269 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-24967 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-24942 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L69-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-09 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L67-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L27-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L69-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-09 |
filingDate | 2005-04-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2011-01-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2f955fd451468e92b36feed643a104f0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_39c741b9c4601f83de381fd1fce56f3e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_83ab5ba5df176f61eca33040d4ef34ed |
publicationDate | 2011-01-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | EP-1741752-B1 |
titleOfInvention | Molded aromatic polycarbonate and resin composition |
abstract | A thin-walled polycarbonate molding which is made of a resin composition comprising 100 parts by weight of (A) an aromatic polycarbonate or a resin consisting mainly of an aromatic polycarbonate, 0.1-200 parts by weight of (B) an inorganic compound, 0.001-10 parts by weight of (C) at least one compound selected among organic acid compounds and organic acid compound derivatives, and 0.001-1 part by weight of (D) at least one metal salt selected among alkali metal salts of organic acids and alkaline earth metal salts of organic acids, at least 50%, in terms of surface area, of the thin-walled polycarbonate molding having a thickness less than 0.7 mm, the thin-walled polycarbonate molding, upon 30-minute standing in an atmosphere of 170°C, having a degree of shrinkage in the molding flow direction, S1 (%), which satisfies the following relationship (1). -60 < S1 < -1 relationship (1) |