http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-1727838-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1f8713f6ace083308920724981592661 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F210-16 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F210-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B3-18 |
filingDate | 2005-03-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e77b0e5682bb53da472c29209d6a39ca http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_91a2a6080e467da71f894ce2282ad168 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_af177e6378bb2ec63b737a7466335c2f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f50913eca66e9a67a69de15bca3bb371 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8fe3d2a53828d5cdff980b769d69bd3a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3713d43b0d4d2e70343952509e7fe7f7 |
publicationDate | 2006-12-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | EP-1727838-A1 |
titleOfInvention | Process for making ethylene interpolymers and interpolymers made thereby; compositions and electrical devices containing such interpolymers |
abstract | The invention relates to a continuous polymerization process for preparing a random ethylene interpolymer with propylene and/or 1-butene which comprises: (A) polymerizing ethylene, and as an α-olefin comonomer propylene and/or 1-butene under continuous random polymerization conditions in the presence of single site catalyst system employing an ionic activator having cyclic ligands shielding a central charge bearing atom, at a temperature of 140° C to 250° C at a conversion of ethylene of 80 to 99% and a comonomer conversion of from at least 30 % and (B) devolatilizing the polymer to provide an ethylene copolymer having a density of from 0.85 to 0.92 g/cm3, an MI of from 0.01 to 100 g/10 min, preferably from 0.1 to 20, and I21/I2 of from 30 to 400. The invention also relates to polymers made such processes containing as α-olefin comonomer propylene and/or 1-butene, having density of from 0.85 to 0.92 g/cm3, an MI of from 0.01 to 100 g/10 min and an I21/I2 of from 30 to 400 obtained by solution polymerization using a transition metal complex as a catalyst and a non-coordinating anion to provide a level of NCA derived residue, as determined by boron content, less than 0.5ppm. as determined by ICP, preferably undetectable by ICP. The polymers may be blended with EP rubber elastomers and be used for electrical cable insulation. |