http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-1693701-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_73ebc284a55d5daf0e209d6186c9e65c |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K2323-021 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02F1-13378 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C14-226 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C14-46 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02F1-133734 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C14-3407 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02F1-1337 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C14-10 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02F1-1337 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C14-46 |
filingDate | 2006-02-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_594840edf8e0117b2287f30afbd82e76 |
publicationDate | 2006-08-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | EP-1693701-A1 |
titleOfInvention | Method of forming inorganic orientation film, inorganic orientation film, substrate for electronic devices, liquid crystal panel, and electronic equipment |
abstract | In a method of forming an inorganic orientation film (200), a target (500) is irradiated with ion beams supplied from an ion beam source (S1) to lead out sputter particles from the target (500), and then the sputter particles are made incident on a matrix (100) to form the inorganic orientation film (200), wherein the film formation is carried out without replacing the whole of the target (500) while carrying out a repair processing for supplementing or recovering a defect of the target (500). The target (500) is formed from a plurality of separable members (510,520) so that only a part of the separable members (510,520) can be selected and replaced, and the repair processing is carried out by replacing a member (510) within the plural separable members on which the defect is produced. According to this method, it is possible to manufacture an inorganic orientation film which is excellent in an orientation characteristic and also excellent in light resistance while effectively using the target. This saves resources and gives fewer burdens on an environment. Further, an inorganic orientation film obtained by the forming method, and a substrate for electronic devices provided with the inorganic orientation film are also provided. Furthermore, a liquid crystal panel provided with the in organic orientation film, and electronic equipment provided with the liquid crystal panel are also provided. |
priorityDate | 2005-02-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 44.