abstract |
The present invention relates to a multimodal polyethylene composition wherein (i) the composition has an MFR 2 of 0.1 to 100 g/10min, (ii) the shear thinning index SHI (1,100) and the log MFR 2 of the composition satisfy the following relation: SHI ( 1 , 100 ) ¥ - 10.58 logMFR 2 [ g / 10 min ] / ( g / 10 min ) + 12.94 , and (iii) the composition has an environmental stress crack resistance ESCR of 10 h or more. Furthermore, the present invention relates to a process for the production of said composition, an injection moulded article, in particular a cap or closure, comprising said composition and to the use of said composition for the production of an injection moulded article. |