http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-1646508-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_5d9f3ca41550d315642580237250c5b0 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B41M5-5236 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B41M5-5254 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B41M5-5218 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B33-26 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41M5-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21H17-67 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41J2-01 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41M5-52 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01B33-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01B33-46 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21H17-33 |
filingDate | 2004-07-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f91012b24fafaf17f4e4b6e3bcb33a13 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_286236af1504e93e667d5eeceafba27f |
publicationDate | 2006-04-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | EP-1646508-A1 |
titleOfInvention | Inkjet recording element |
abstract | The present invention relates to an inkjet recording element having very good dye keeping properties in time. Said inkjet recording element comprises a support and at least one ink-receiving layer, said ink-receiving layer comprising at least one hydrosoluble binder and at least one aluminosilicate polymer obtainable by a preparation method consisting in treating an aluminum halide with a mixture of at least one silicon alkoxide only having hydrolyzable substituents and at least one silicon alkoxide having a non-hydrolyzable substituent, with an aqueous alkali in the presence of silanol groups, the aluminum concentration being maintained less than 0.3 mol/l, the Al/Si molar ratio being maintained between 1 and 3.6 and the alkali/Al molar ratio being maintained between 2.3 and 3; and then stirring the resulting mixture at ambient temperature in the presence of silanol groups for long enough to form the hybrid aluminosilicate polymer. The ink-receiving layer also comprises inorganic particles. |
priorityDate | 2003-07-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 83.