http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-1614717-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_0ddb9f3656270bc5410be3679322fead |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K2200-0657 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L71-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K3-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G65-336 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G65-2663 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K3-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G65-336 |
filingDate | 2004-03-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_47d51e84906a3760bb1f4abfe7588d59 |
publicationDate | 2006-01-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | EP-1614717-A1 |
titleOfInvention | Curable composition |
abstract | The present invention provides a curable composition comprising a reactive silicon group-containing polyoxyalkylene polymer which is obtained by reacting a polyoxyalkylene polymer (A) having a molecular weight distribution of 1.6 or less, a number average molecular weight of 15,000 to 50,000, and 0.8 or more reactive groups, on average, per molecule thereof with an organic compound (B) having in the molecule thereof a reactive silicon group and a functional group capable of reacting with the reactive groups of the polymer (A) in a proportion of 0.8 to 1.5 molecules of the organic compound (B), on average, per molecule of the component (A), a filler (C) and a curing catalyst (D); further in which, in the liquid components contained in the curable composition, the ratio y/x of the content y (wt%) of a component having no reactive silicon group and the content x (wt%) of a component having at least one reactive silicon group is 0.4 or less; and further in which the composition comprises a plasticizer in an amount of 10 parts by weight or less in relation to 100 parts by weight of the reactive silicon group-containing polyoxyalkylene polymer. The curable composition of the present invention improves the staining property of the cured product thereof, ensures favorable mechanical properties favorable for a sealant such as low stress and high elongation, and is also satisfactory in workability. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-101501137-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-2510029-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/DE-102013216787-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9353225-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-2036938-A4 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-2053092-A4 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-2036938-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-2840087-A1 |
priorityDate | 2003-04-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 440.