Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d63db43defeda5c11229cc168c4e1d81 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D3-107 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D5-005 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D3-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D3-141 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D7-546 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D7-14 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D5-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D3-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D3-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D3-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-14 |
filingDate |
2004-01-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2009-07-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3e24d1bfaf415004f8c3dada1431b34c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_23985b97a4f41fc5e34250cbe590cf79 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b0439e047f1028508c06f3bf9451051f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d88948425a0730c1a18e4ae0f3988b15 |
publicationDate |
2009-07-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
EP-1594629-B1 |
titleOfInvention |
Use of a process for making a multilayer coating for making and/or repairing a (serial) car paint |
abstract |
The invention relates to a method for producing a multilayer coating consisting in applying another coating substance (B) to a first coating (A) and in hardening said substance. Said first coating (A) is selected and/or modified and/or the coating substance (B) is selected in such a way that a quotient (Q) between the surface energy of the second coating substance (B) and the surface energy of the first coating (A) is equal to ≤1. The use of the inventive method is also disclosed. |