Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_558b57c8c61df7eb6dde16dab37f4ab4 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G01N2203-0017 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G01N2203-0268 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G01N2291-0231 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G01N2291-044 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G01N2291-0421 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G01N2291-102 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G01N2291-015 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G01N29-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G01N29-11 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G01N19-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G01N29-4472 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G01N3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G01N3-02 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G01N19-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G01N29-11 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G01N3-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G01N29-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G01N29-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G01N29-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G01N29-04 |
filingDate |
2005-01-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_20655e5a02fbe5f86c4023afac078d69 |
publicationDate |
2005-11-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
EP-1562034-A9 |
titleOfInvention |
Method for measuring the adhesion of a coating on a substrate by acoustic coupling of the transducers by means of a thin gel layer |
abstract |
Method for measuring the adhesion of a coating (2) to a substrate (1), characterized in that the measurement is made in the air and in that an ultrasonic transducer (3) is applied to the substrate ( 1) by means of a thin layer (7) of gel and a given quality factor is calculated by the ratio between the amplitudes of the echoes associated with the first two reflections on the interface substrate (1) - coating (2) after crossing of the substrate (1) or on the interface coating (2) - air after passing through the substrate (1) and the coating (2). |