http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-1553104-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_bb4ee28d43b5e8d4a3c5141fa9bcfeb0 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F2-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F214-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F214-22 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F14-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F214-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F214-18 |
filingDate | 2003-07-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e2847469d64eca8ff131fe73cc1d253a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f78cb22a2a0df09be17add56c64fc82c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5f1ee5dd4bdb633b01a8dfba098529d4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_22fe5ecbc43d5bba2f5956db6d46f872 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b9a989e95003e174a29b751e0aa93c61 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_893b2aee4c6b723350f8e0488acbc4d7 |
publicationDate | 2005-07-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | EP-1553104-A1 |
titleOfInvention | Process for producing fluoropolymer |
abstract | The present invention provides a process for preparing anfluorine-containing polymer having few branched chains and littlenweight change in high temperatures, which is a new process whereinncomposition distribution substantially does not occur. The fluorine-containingnpolymer is prepared by a batch copolymerization processnconducted under conditions of reduced temperature of at least 0.95 andnreduced pressure of at least 0.80 of the critical constant calculated fromncritical temperature, critical pressure and composition ratio of eachnmonomer in the gaseous phase of the reaction vessel using the Peng-Robinsonnformula; wherein when the number of monomer componentsnin the target polymer is represented as n (n is an integer of 2 or larger),nthe name of each monomer component is represented as A 1 , A 2 , ...A n ,nthe weight percentage of each monomer component A 1 , A 2 , ...A n of thentarget polymer composition is represented as a 1 , a 2 , ...a n (%) (a satisfiesn a n = 100), the weight percentage of each monomer component of theninitial monomer composition is represented as a' 1 , a' 2 , ...a' n (%) (a'nsatisfies a n ' = 100 and a' 1 , a' 2 , ...a' n is determined in a constantnmanner depending on predetermined polymerization conditions) andnspecific gravity of the gaseous phase monomers whennpolymerizing/ specific gravity of the target polymer is represented as B,nthe composition weight ratio of additional monomers is calculated forneach monomer from the formulan (a 1 -a' 1 × B) : (a 2 -a' 2 × B)...(a n -a' n × B) nin the order of components A 1 , A 2 , ...A n , and additional monomersncontaining additional monomers in the composition weight ratio ofnadditional monomers are added. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/FR-2896250-A1 |
priorityDate | 2002-07-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 146.