http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-1511782-B1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_0efa077d881a96aeb1e29b21ef1bbb58 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J151-003 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F265-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L51-003 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F257-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F285-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F291-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F265-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J151-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F285-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L51-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F257-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F291-00 |
filingDate | 2003-05-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2007-07-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_01739c0c898da7ad3ec5c72ea7f3f0f3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_652326353d60b59d830d242118b1bc3a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_96a02d18aecaae1b8c5d76082b11bc44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ce6b9f6bef9d49e78e8568a739f50621 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9be853571f590a22a78fb753d5f0c436 |
publicationDate | 2007-07-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | EP-1511782-B1 |
titleOfInvention | Method for producing an aqueous polymer dispersion |
abstract | The invention relates to a method for producing an aqueous polymer dispersion having a polymer solids content of >=50% by weight by carrying out the radically initiated aqueous emulsion polymerization of ethylenically unsaturated compounds (monomers). The inventive method is characterized in that: a) a mixture is provided in a polymerization vessel and contains a partial quantity 1 consisting of: deionized water, 0.001 to 0.5 parts by weight of a polymer with a weighted average particle diameter of <=100 nm; 0.0001 to 0.1 parts by weight of dispersants, and 0.5 to 10 parts by weight of monomers, and the monomers are polymerized with a conversion of >=80% [polymerization step A], and; b) afterwards, a monomer emulsion containing partial quantity 2, which consists of deionized water, 0.1 to 5 parts by weight of dispersants and 90 to 99.5 parts by weight of monomers, is fed under polymerization conditions to the obtained reaction mixture [polymerization step B], whereby; c) the total amount of the monomers used for the polymerization is equal to 100 parts by weight, and the total amount of deionized water is <=100 parts by weight. |